1. SF型浮选机
钼矿浮选机推荐选择XJK型、SF型或JJF型浮选机。是适合的
2. sf型浮选机技术参数
类别规格型号有效容积(mЗ)处理能力(mЗ/min)主轴刮板槽体尺寸(Mm)单槽重量(kw) 功率(kw)转速(r/min)转速(r/min)功率(kw) XJ型浮选机XJ-0.350.350.18-0.41.5483251.1700×700×700460XJ-0.620.620.3-0.93.0400251.1900×820×850980 XJ-1.11.10.6-1.65.5330251.11100×1100×10001390 XJ-2.82.81.5-3.511280251.11750×1600×11002430 XJ5.85.85.0-7.022240251.52200×2200×12003533 SF型浮选机SF-0.370.370.2-0.41.5352251.1700×700×750468SF-0.70.70.3-0.93400251.1900×820×950600 SF-1.21.20.6-1.65.5330251.11100×1100×11001873 SF-2.82.81.5-3.511268251.11750×1600×11502538 SF-442.0-4.015220251.51850×2050×12002838 SF-884.0-8.030191251.52200×2900×14004129 SF-10105.0-1030191251.52200×2900×17004486 SF-20205.0-2030×2191251.5×22850×3800×20009828 JJF型浮选机JJF-221.0-3.07.5443251.51400×1400×11001670JJF-442.0-4.011305251.51600×1400×11002350 JJF-884.0-8.022233251.52200×2900×14004500 JJF-10105.0-1022233251.52200×2900×17004820 JJF-16165.0-1627180251.52850×3800×17008000 JJF-20205.0-2037180251.52850×3800×200010500
3. sf型浮选机尾矿箱
如果跑的煤是大于0.5mm的颗粒这也算正常,如果跑的是小于0.5mm颗粒的煤就不太正常了。
如果是大于0.5mm的颗粒可以通过加装分级筛,如果跑的是小于0.5mm颗粒可以更换浮选药剂和改进浮选工艺试一试,如有不明白可以hi我。
4. 磁选机浮选机
干式磁选机是可以选别湿度在5%以下的矿石,例如锰矿干选机,褐铁矿干选机,钾长石干选机等。
通常干选机分为上筒下辊干选机,双辊干选机,一筒三辊干选机和双筒三辊干选机等。
湿式磁选机选矿过程必须依靠水为介质的磁选机,湿式磁选机分为弱磁湿式磁选机,中磁湿式磁选机和强磁湿式磁选机等,而根据类型又可以分为永磁湿式磁选机和电池湿式磁选机等。
这两种磁选机目前主要运用在铁矿磁选和锰矿的磁选上。无论是强磁湿式磁选机还是强磁干式磁选机,天创磁力是一个非常专业的设备生产厂家。
5. 浮选机选型
1.优先浮选。一般是先浮铜,然后再浮硫。致密块状含铜黄铁矿,矿石中黄铁矿的含量相当高,常采用高碱度、高黄药用量的方法浮铜抑制黄铁矿。其尾矿中主要是黄铁矿,脉石很少,所以尾矿便是硫精矿。对于浸染状铜硫矿石,采用优先浮选流程,浮铜后的尾矿要再浮硫,为了降低浮硫时硫酸的消耗及保证安全操作,浮铜时,尽量采用低碱度的工艺条件。
2.混合-分离浮选。对于原矿含硫较低,铜矿物易浮的铜硫矿石选用这种流程较有利。铜硫矿物先在弱碱性矿将中进行混合浮选,混合精矿再加石灰在高碱性矿浆中进行铜硫分离。
3.半优先混合-分离浮选。半优先混合-分离浮选是以选择性好的酯类作为半优先浮铜作业的捕收剂,先浮出易浮的铜矿物,得到部分合格的铜精矿,然后再进行铜硫混合浮选,所得的铜硫混合精矿使用浮铜抑硫的分离浮选。这种分离流程,避免了高石灰用量下对易浮铜矿物的抑制,也不需要耗大量硫酸活化黄铁矿。生产实践表明:这种流程结构合理,操作稳定,指标好,具有尽早回收目的矿物的特点。此信息来源于:www.gyxxjx.com